Hardware manual
Spectrum Z™510 3D Printer Hardware Manual Post-Processing the Part
www.3dpuser.com
37
10/1/07 All Rights Reserved
7.5 Drying the Part
Although the part can be handled when it is not completely dried, the part reaches full strength when dried.
Placing the part in an oven at temperatures less than 200
° F (93°C) for 2-4 hours will dramatically increase
the strength of the part. This is only recommended for high definition composite powders. If using the
removable build plate, remove the part from the build plate before placing in the oven.
Click the following links for additional information on our 3DP™ User website regarding:
Accessories
Frequently Asked Questions regarding Ovens
Despatch Oven General Description
7.6 Part Infiltration
All parts can be infiltrated with a variety of resins to produce a range of material properties. As an early
stage design tool, it may not be necessary to infiltrate the parts at all. However, the true versatility of the
Z510 3D Printer System is derived from the variety of material properties that can be achieved by applying
one of our infiltration materials to parts that will be exposed to a variety of product testing environments.
For additional information on how customers are utilizing our line of infiltration products visit our 3DP™
User website at www.3dpusers.com
.
For an updated infiltrant product selection guide, please visit the 3DP™ User Website at
www.3dpusers.com
, or click one of the links in the table below.
To learn more about finishing moving parts, finishing color parts, and finishing a part using the dipping
method, click Application Resources
and view additional applications information on the 3DP™ User web-
site.
INFILTRANTS MATERIAL SYSTEM APPLICATION
Wax High Composite Material Dip
Z-Bond™ Cyanoacrylate High Composite Material Brush or Drizzle
Z-Max™ Epoxy High Composite Material Spray or Brush