Specifications
16
Soldering Investments
For Low- and High-Fusing Precious Metals
Physical Properties
Soldering Investment Hi-Heat
Water/Powder Ratio 24 mL/100 g 28 mL/100 g
Working Time 2–3 minutes 2–4 minutes
Ready for Dewaxing (Minimum) 15 minutes 20 minutes
Setting Expansion 0.20% 0.20%
Thermal Expansion 700° C (1,300° F) 0.60% 1.00%
Compressive Strength, Wet (2 hours) 1,200 psi (9 MPa) 300 psi (2 MPa)
Soldering Investment
For all soldering purposes
Multi-purpose Soldering Investment is
ideal for soldering all types of dental
alloys, including chrome-cobalt. Its
ne texture mixes readily with water
to a smooth, stackable consistency
that invests easily. Heat-shock
resistance and high strength enable it
to withstand being dried out or ushed
with boiling water. This improved
soldering investment is strong, yet
easy to devest.
Item No. Description
01473 2 kg (4 1/2 lb.) Package
01503 11 kg (25 lb.) Carton
is ideal for any soldering job that
requires the use of an oxygen-gas
torch, or where an unusually ne
and smooth soldering investment is
wanted. Excellent for use with high-
fusing ceramic alloys for both the
pre- and post-soldering technique.
Can also be used for soldering
precision attachments.
Hi-Heat
For high-fusing precious metals
• Flows freely into the smallest
crevice
• Stacks and molds easily
• Sets moderately fast
• Trims smoothly
• Withstands rapid drying out
Hi-Heat Soldering Investment is
a gypsum-bound investment that
Item No. Description
01546 2 kg (4 1/2 lb.) Package
01562 11 kg (25 lb.) Carton