Installation Guide
©2012 Titan Florida TAR-2138-04 2/12
ACCESSORY PRODUCTS
The water and aggregate used in the mixing process
should be free of any substance that could adversely
affect the hardened masonry or any metal accessories
used in the system.
APPLICATION
Estimated coverage per bag of material in square feet.
No allowance for waste, aggregate size or field
conditions. Actual coverage will vary.
*Sand to Cement ratio.
CAUTION
Causes skin irritation, injurious to eyes.
Contains Portland Cement. Freshly mixed
cement, mortar, concrete or grout may
cause skin injury. Avoid contact with skin
where possible and wash exposed skin
areas promptly with water. If any cement
or cement mixtures get into the eyes, rinse
immediately and repeatedly with water for
15 minutes and get prompt medical attention.
KEEP OUT OF THE
REACH OF CHILDREN
Titan Florida
11000 NW 121st Way
Medley, FL 33178
For additional information or to obtain
Material Safety Data Sheets, please visit
www.titanamerica.com or call Customer
Service at (800) 226-2057.
STUCCO CEMENT
RECOMMENDED USES
Titan America
®
Stucco Cement is specifically designed for interior and exterior applications of
Portland Cement based plasters. It is common to see this product applied over wire lath, con-
crete unit masonry and cast-in-place concrete. Additional additives may be required to assist
in the bonding of the Stucco to certain substrates such as cast-in-place or pre-cast concrete.
SPECIFICATIONS AND QUALITIES
Titan America
®
Stucco Cement is manufactured by inter-grinding Portland Cement Clinker
(meeting ASTM C-150), Gypsum and Limerock. Water repellent and air-entraining admix-
tures are added during the manufacturing process to assist with workability and board life.
Titan America
®
Stucco Cement meets or exceeds the requirements of ASTM C-91.
Titan America
®
Stucco Cement when mixed with masonry sand (ASTM C-144) and tested
according to ASTM C-270 will produce a mortar that complies with those requirements.
Titan America
®
Stucco Cement, when mixed in accordance with ASTM C-1328,
will produce stucco cement that meets or exceeds the requirements of that Standard.
INSTRUCTIONS
Titan America
®
Stucco Cement
• No allowance for waste, aggregate size or field conditions.
• One bag of Titan America
®
Stucco Cement is approximately one cubic foot by volume.
• Approximately six #2 shovels of damp, loose sand equals one cubic foot by volume.
CEMENT PREPARATION
Titan America
®
Stucco Cement will not perform as designed if the mixing instructions are
not followed correctly. It is important to ensure that the product does not dry out prema-
turely; this condition can affect the overall strength and durability of the finished product.
The cement should be mixed only with clean sand and potable water unless prior sampling
shows potential job materials will produce the desired mortar.
Mix in a mechanical mixer as follows:
1) Add approximately 2/3 of the potable water required.
2) Add 1/2 of the sand required (ASTM C-144 approved).
3) Add Fiber prior to the addition of cement if applicable.
4) Add Titan America
®
Stucco Cement.
5) Add the remainder of the sand (ASTM C-144 approved).
6) Add enough potable water to bring mortar to desired consistency.
7) Allow mortar to mix 5 minutes after the introduction of the last ingredient.
Short mixing or overloading with sand can produce a lower mortar quality.
WALL PREPARATION
All surfaces to be plastered must be clean of contaminants and/or any debris, including
excess uncured mortar from block masonry that may affect the Stucco Cement from
achieving adequate bond. It is recommended, prior to any application, to determine
whether there is a need for a bonding agent to assist in the attachment of the Stucco
Cement. Concrete Block applications should be uniformly wet (fogged) just prior to
application of the first and each succeeding plaster coat. To obtain the best results,
some moisture should be maintained in the stucco (by fogging if necessary) for the first
few days after application.
Scratch (Capa Inicial) 1 Bag 2
1
/2
: 4 15–24
Brown (Segunda Capa) 1 Bag 3 : 4 18–24
Finish (Capa Final) 1 Bag 2 : 3 12–18
Plaster Coats
Titan America
®
Stucco
80 lb. bags
Parts/Partes
Cement : Sand
Cemento : Arena
Shovels/Part
Palas/Parte
Sand/Arena
PROPORTIONAL MIXING GUIDELINES
3/8” 3/8” 5/8” 7/8”
2
1
/2
: 1 112 84
67 48
3 : 1 128 96
77 55
3
1
/2
: 1
144
108
87 62
4 : 1
160
120
96 69
Parts*
Partes
Thickness/Grueso