Datasheet

DataSheet
30W, Single Output
VER:00 Page 44 of 46 Issued Date:2009/03/02
Soldering and Reflow Consideration
Lead free wave solder profile for PXE30-xxWSxx DIPtype
Zone Reference Parameter
Preheat zone Rise temp. speed: 3°C / sec max.
Preheat temp. : 100~130°C
Actual heating Peak temp. : 250~260°C
Peak time (T1+T2 time) : 4~6 sec
Reference Solder: Sn-Ag-Cu/Sn-Cu
Hand Welding: Soldering iron-Power 90W
Welding Time: 2-4 sec
Temp.: 380-400 °C
Packaging Information
12 PCS per TUBE