Soldering and Reflow Consideration
Lead free wave solder profile for PXD20-xxSxx DIPtype
Zone Reference Parameter
Preheat zone Rise temp. speed : 3°C / sec max.
Preheat temp.: 100~130°C
Actual heating Peak temp. : 250~260°C
Peak time (T1+T2 time) : 4~6sec
Reference Solder:Sn-Ag-Cu/Sn-Cu
HandWelding: Soldering iron- Power90W
Welding Time: 2-4 sec
Temp.:380-400 °C