SDS
SAMSUNG SDI Co., Ltd.   
Date: January 1, 2016    Revision no.: 00 
MODEL: INR18650-20Q     
Page 4 of 11 
25038-59-9 
Polyethylene terephthalate 
0.753 
24937-79-9 
1,1-Difluoroethylene polymer 
0.5 
1333-86-4 
Carbon black 
0.5 
24968-12-5 
Poly(oxy-1,4-butanediyloxycarbonyl-1,4-phenylenecarbonyl) 
0.451 
9003-07-0 
Polypropylene 
0.402 
25053-09-2 
2-Propenoic acid, 2-methyl-, methyl ester, polymer with 
1,3-butadiene and ethenylbenzene 
0.32 
114435-02-8 
4-Fluoro-1,3-dioxolan-2-one 
0.316 
35239-19-1 
2-Propenoic acid, polymer with butyl 2-propenoate, ethenyl 
acetate and 2-ethylhexyl 2-propenoate 
0.3 
9004-32-4 
Sodium carboxymethyl cellulose 
0.21 
14807-96-6 
Talc 
0.1 
26023-21-2 
Poly[N,N`-(1,4-phenylene)-3,3`,4,4`-benzophenonetetracarboxylic 
imide/amic acid] 
0.1 
13463-67-7 
Titanium dioxide 
0.1 
9003-56-9 
ABS resin 
0.05 
81-77-6 
Ci 69800 
0.02 
7440-21-3 
Silicon 
0.011 
25038-81-7 
1H,3H-Benzo[1,2-c:4,5-c`]difuran-1,3,5,7-tetrone, polymer with 
4,4`-oxybis[benzenamine] 
0.01 
7439-96-5 
Manganese 
0.01 
7439-95-4 
Magnesium 
0.01 
7440-66-6 
Zinc 
0.002 
57455-37-5 
Ultramarine blue 
0.0015 
7440-32-6 
Titanium 
0.0014 
1317-80-2 
Rutile (TiO2) 
0.001 
7440-47-3 
Chromium 
0.0005 
7723-14-0 
Phosphorus 
0.0002 
7440-62-2 
Vanadium 
0.00006 
Because of the cell structure the dangerous ingredients will not be available if used properly. 
During charge process a lithium graphite intercalation phase is formed.   
4. First Aid Measures 
Description of first aid measures 
The hazardous components of this cell or battery are contained within a sealed unit. The following measures are only 
applicable if exposure has occurred to components when a cell or battery leaks, is exposed to high temperatures or is 
mechanically, electrically or physically abused/damaged. The hazardous contents are caustic alkaline electrolytes 