SDS
SAMSUNG SDI Co., LTD   
Date: January 1, 2015     Revision no.: 02 
MODEL INR18650-25R 
Page 3 of 9 
616-38-6 
dimethyl carbonate 
< 5% 
623-53-0 
Ethyl methyl carbonate 
< 2% 
7782-42-5 
Graphite 
< 2% 
26023-21-2 
imide resin 
< 1% 
7439-89-6 
Iron 
< 15% 
554-13-2 
lithium carbonate 
< 1% 
21324-40-3 
lithium hexafluorophosphate(1-) 
< 2% 
12057-17-9 
Lithium manganese oxide 
< 4% 
12325-84-7 
Lithium Nickel Oxide 
< 17% 
12031-65-1 
Lithium nickelate 
< 7% 
14283-07-9 
lithium tetrafluoroborate, anhydrous 
< 1% 
244761-29-3 
Lithium-bis-oxaiatoborate 
< 1% 
7439-95-4 
Magnesium 
< 1% 
7439-96-5 
Manganese 
< 1% 
7440-02-0 
Nickel 
< 1% 
16812-54-7 
Nickel monosulfide 
< 1% 
7786-81-4 
Nickel sulfate 
< 1% 
7791-20-0 
nickel(ii) chloride hexahydrate 
< 1% 
24968-12-5 
poly(1,4-butylene terephthalate) 
< 1% 
9002-88-4 
Polyethylene 
< 3% 
7440-21-3 
Silicon 
< 1% 
9003-55-8 
Styrene, butadiene copolymer 
< 1% 
14807-96-6 
Talc (Mg3H2(SiO3)4) 
< 1% 
13463-67-7 
titanium dioxide 
< 1% 
4325-85-3 
Tris(trimethylsilyl)borate 
< 1% 
Full text of each relevant R phrase can be found in heading 16. 
Further Information   
For information purposes: 
(*) Main ingredients: Lithium hexafluorophosphate, organic carbonates 
Because of the cell structure the dangerous ingredients will not be available if used properly. 
During charge process a lithium graphite intercalation phase is formed. 
4. First Aid Measures 
General information 
The following first aid measures are required only in case of exposure to interior battery components after 
damage of the external battery casing. 
Undamaged, closed cells do not represent a danger to the health. 
After inhalation   
Ensure of fresh air. Consult a physician.   









