Instruction Manual
• • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • •
I N S T R U C T I O N M A N U A L • H A N D H E L D W E L D E R S
31
A P P L I C A T I O N S – S P O T W E L D I N G
During spot welding, the horn tip penetrates through the top sheet and
e
nters the bottom sheet to a depth of one half the top sheet thickness. The
displaced molten plastic is shaped by a cavity in the tip to create an annular
formation around the weld. Simultaneously, the molten plastic displaced
from the second sheet flows into the preheated area and forms a permanent
molecular bond. Large thermoplastic parts and applications with hard to
reach joining surfaces can easily be welded together using an ultrasonic spot
welder and standard replaceable tips.
STANDARD THREADED TIPS FOR SPOT WELDING
ORDERING INFORMATION
Specify tip required using code letter.
Example:
Spot weld tip “SA” indicates a tip used for spot welding – 1/32" thick
material.
• • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • • •
BEFORE
A
FTER
PLASTIC
HORN
PLASTIC
3t
t
1.5t
Material Thickness TIP
CODE
inches mm
LETTER
1/32 0.793 SA
3/64 1.190 SB
1/16 1.587 SC
5/64 1.984 SD
3/32 2.381 SE
7/64 2.778 SF
SPOT WELDING
Go To Top Of Document