Technical Specifications

URETHANE
TECHNICAL DATA
RO-71
HIGH PERFORMANCE
9800 SYSTEM DTM URETHANE MASTIC
3
PERFORMANCE CHARACTERISTICS
SYSTEM TESTED
9800 System DTM Urethane Mastic.
For chemical and corrosion resistance, see the Rust-Oleum Industrial
Brands Catalog (Form #275585).
PENCIL HARDNESS
METHOD: ASTM D3363
RESULT: F-H
CONICAL FLEXIBILITY
METHOD: ASTM D522
RESULT: 32%+
CYCLIC PROHESION
Rating 1-10, 10=best
METHOD: ASTM D5894, 4 cycles, 1,344 hours
RESULT: 10 per ASTM D714 for blistering
RESULT: 10 per ASTM D610 for rusting
IMPACT RESISTANCE (direct/reverse)
METHOD: ASTM D2794
RESULT: 160/160 in.lbs.
TABER ABRASION
METHOD: ASTM D4060, CS-17 wheels, 1,000 gram load,
1000 cycles
RESULT: 74 mg loss
GLOSS (60°)
METHOD: ASTM D523
RESULT: 83% (colorwhite)
ACCELERATED WEATHERING (% gloss retention)
METHOD: ASTM D4587, QUV Type A bulb, 1,551 hours
RESULT: 95% gloss retention (colorwhite)
MOISTURE PERMEABILITY
METHOD: ASTM D1653
CONDITIONS: 73°F 50% RH 3.1 mils WFT
RESULTS: WVT-2.73 g/m
2
/24 hours
WVP-0.26 g/m
2
/24 hours/mm Hg