NOTES
1.
1)
This floor life is only applicable when the environment conforms to IPC/JEDEC J-STD-033.
2. To avoid blistering, layer separation and other soldering issues, it is forbidden to expose the modules
to the air for a long time. If the temperature and moisture do not conform to IPC/JEDEC J-STD-033 or
the relative moisture is over 60%, It is recommended to start the solder reflow process within 24 hours
after the package is removed. And do not remove the packages of tremendous modules if they are not
ready for soldering.
3. Please take the module out of the packaging and put it on high-temperature resistant fixtures before
the baking. If shorter baking time is desired, please refer to IPC/JEDEC J-STD-033 for baking
procedure.
8.2.
Manufacturing and Soldering
Push the squeegee to apply the solder paste on the surface of stencil, thus making the paste fill the stencil
openings and then penetrate to the PCB. The force on the squeegee should be adjusted properly so as to
produce a clean stencil surface on a single pass. To ensure the module soldering quality, the thickness of
stencil for the module is recommended to be 0.130.15 mm. For more details, please refer to document
[4].
It is suggested that the peak reflow temperature is 238246 ºC, and the absolute maximum reflow
temperature is 246 ºC. To avoid damage to the module caused by repeated heating, it is strongly
recommended that the module should be mounted after reflow soldering for the other side of PCB has
been completed. The recommended reflow soldering thermal profile (lead-free reflow soldering) and
related parameters are shown below.
Tem p. (°C )
R eflow Z one
M ax slop e:
C ooling dow n slope:
246
2 to 3°C /s
C
-1.5 to -3°C /s
238
220
200
B
D
S oak Z one
150
100
A
M ax slop e: 1 to 3°C /s
Figure 46: Recommended Reflow Soldering Thermal Profile