Information
Property
Testing Method
Typical Value
Young’s modulus (X-Y)
ISO 527, GB/T 1040
2379 ± 157 MPa
Young’s modulus (Z)
1965 ± 136 MPa
Tensile strength (X-Y)
ISO 527, GB/T 1040
43.8 ± 0.8 MPa
Tensile strength (Z)
32 ± 1.8 MPa
Elongation at break (X-Y)
ISO 527, GB/T 1040
6.7 ± 0.6 %
Elongation at break (Z)
1.65 ± 0.2 %
Bending modulus (X-Y)
ISO 178, GB/T 9341
3206 ± 108 MPa
Bending modulus (Z)
N/A
Bending strength (X-Y)
ISO 178, GB/T 9341
73.4 ± 2.1 MPa
Bending strength (Z)
N/A
Charpy impact strength (X-Y)
ISO 179, GB/T 9343
10.3 ± 0.4 kj/m
2
Charpy impact strength (Z)
6.7 ± 1.4 kj/m
2
Printing temperature
260 °C
Bed temperature
90 °C
Shell
2
Top & bottom layer
4
Infill
100%
Environmental temperature
50 – 70 (recommended) (˚C)
Cooling fan
OFF