Technical Bulletin
18900 Panduit Drive
Tinley Park, IL 60487
Customer Service: 800-777-3300
TDS:
Effective Date:
Revision:
GMNT
16JUL12
6
Technical Data Sheet
Page 2 of 5 2007 PANDUIT Corp
TDS: GMNT
®
*3000 hours equates to 5 years of assimilated outdoor UV exposure.
CHEMICAL/SOLVENT RESISTANCE:
The testing was conducted at room temperature. Samples were thermal transfer printed with Panduit
Resin ribbon on Panduit printer.
Chemical/Solvent
7 DAY IMMERSION
DIP TEST
RUB TEST
30% Sulfuric acid
1
1
1
10% Sulfuric acid
1
1
1
30% Hydrochloric
acid
1
1
1
10% Hydrochloric
acid
1
1
1
50% Sodium
Hydroxide
2
1
1
10% Sodium
Hydroxide
3
1
1
Methyl Ethyl Ketone
3
3
3
Acetone
3
3
3
1:1:1 Trichloroethane
2
1
3
Isopropyl Alcohol
3
1
1
ASTM#3 Oil
1
1
1
SAE 30 Oil
1
1
1
Alconox
1
1
1
Toluene
2
1
3
Mineral Spirits
1
1
1
Glacial Acetic Acid
3
3
3
Diesel Fuel
1
1
1
10% Sodium
Chloride
1
1
1
Water
1
1
1
Gasoline
1
1
1
1 = No change 2 = Slight failure in Legibility 3 = Failure in Legibility
7 Day Immersion – Immersed in reagent for 7 days
Dip Test - Five 10 minute dips in reagent followed by 30 minute recovery
Rub Test - Rubbed sample for 1 minute with swab soaked in reagent
Marking Performance:
MIL-M-81531: Print still legible after 20 eraser rubs with hard hand pressure.