Phau Ntawv Qhia

20
|
nVent.com/RAYCHEM
F
F
XTV, KTV, HTV, VPL
A
B
XTV, KTV, HTV, VPL
16
17
ENGLISH
Important note: Heat shrink technique for S-40 kits Steps 18 and 21
Heat gun power for optimal shrinking time - 3000 W or greater is
recommended. Lower power heat guns may work, but may require
more time.
Recommended heat gun temperature: 600-650°C
1. Set heat gun at recommended temperature, or as close as possible,
and maximum air flow.
2. Starting in the centre, hold heat gun in one position over the
translucentheatshrinktubinguntilitturnsclear(+/–1 min). Then
slowly move the heat gun around all sides until the heat shrink turns
clear in this segment.
3. Slowly move to an adjacent translucent position on one half of the
splice and repeat for this next segment.
4. Slowly continue along the length of heat shrink, rotating the heat gun
at each segment until both halves are complete. Installation can take
several minutes per piece of heat shrink tubing.
5. Keep heat gun as close as possible to heat shrink (5 mm) but do not allow
it to touch cable or heat shrink (to avoid burning and damaging materials).
DE,FR,NL,NO,SV,DA,FI,IT,ES,PL,RU,CZ,HU,CRO:page22-27