Operating instructions

4 Description of control M200 / M210 (optional)
4/17
4.9.4 MIG spot-welding function sequence
t
I
t
t
Fig. 4/7; MIG spots
Spot-welding starts
Torch trigger is operated and held
Shielding gas is expelled (gas pre-flows).
Wire feed motor runs at “creep speed”.
Arc ignites after the wire electrode makes contact with the workpiece, welding current flows.
Changeover to pre-selected WF speed.
Wire-feed motor stops after the selected spotting time expires.
Arc is extinguished after the set wire burn-back time elapses.
Gas post-flow time elapses.
End spot-welding
Spot-welding ends when the pre-selected spotting time expires.
Early ending of spot-welding with the release of the torch trigger.
Release torch trigger: spot-welding can be resumed.