SDS
SAMSUNG SDI Co., LTD
Date: January 1, 2015 Revision no.: 02
MODEL ICP595265A
Page 3 of 9
7439-95-4
Magnesium
< 1 %
14283-07-9
Borate(1-), tetrafluoro-, lithium
< 1 %
77804-81-0
Butanamide,
2,2`-[1,2-ethanediylbis(oxy-2,1-phenyleneazo)]bis[N-(2,3-dihydro-2-oxo-1H-benzi
midazol-5-yl)-3-oxo-
< 1 %
26023-21-2
Poly[N,N`-(1,4-phenylene)-3,3`,4,4`-benzophenonetetracarboxylic imide/amic
acid]
< 1 %
Full text of each relevant R phrase can be found in heading 16.
Further Information
For information purposes:
(*) Main ingredients: Lithium hexafluorophosphate, organic carbonates
Because of the cell structure the dangerous ingredients will not be available if used properly.
During charge process a lithium graphite intercalation phase is formed.
Mercury content: Hg < 0.1mg/kg
Cadmium content: Cd < 1mg/kg
Lead content: Pb< 10mg/kg
4. First Aid Measures
General information
The following first aid measures are required only in case of exposure to interior battery components after
damage of the external battery casing.
Undamaged, closed cells do not represent a danger to the health.
After inhalation
Ensure of fresh air. Consult a physician.
After contact with skin
In case of contact with skin wash off immediately with plenty of
water. Consult a physician.
After contact with eyes
Rinse immediately with plenty of water, also under the eyelids, for at least 15
minutes. Seek medical treatment by eye specialist.
After ingestion
Drink plenty of water.
Call a physician immediately.
5. Fire Fighting Measures
Suitable extinguishing media
Cold water and dry powder in large amount are applicable.
Use metal fire extinction powder or dry sand if only few cells are involved.
Special hazards arising from the chemical