SDS
SAMSUNG SDI Co., LTD   
Date: January 12, 2015     Revision no.: 01 
MODEL ICR18650-22P 
Page 3 of 9 
68604-67-1 
Fatty acids, coco polymers with benzoic acid, 
pentaerythritol and phthalic anhydride 
< 1% 
7782-42-5 
Graphite 
< 17% 
7439-89-6 
Iron 
< 15% 
554-13-2 
lithium carbonate 
< 1% 
21324-40-3 
lithium hexafluorophosphate(1-) 
< 2% 
12057-17-9 
Lithium manganese oxide 
< 19% 
12031-65-1 
Lithium nickelate 
< 13% 
14283-07-9 
lithium tetrafluoroborate, anhydrous 
< 1% 
244761-29-3 
Lithium-bis-oxaiatoborate 
< 1% 
7439-96-5 
Manganese 
< 1% 
108-38-3 
m-xylene 
< 1% 
7440-02-0 
Nickel 
< 1% 
16812-54-7 
Nickel monosulfide 
< 1% 
7786-81-4 
Nickel sulfate 
< 1% 
95-47-6 
o-xylene 
< 1% 
9002-88-4 
Polyethylene 
< 3% 
9003-07-04 
Polypropyllene 
< 1% 
106-42-3 
p-xylene 
< 1% 
7440-21-3 
Silicon 
< 1% 
9003-55-8 
Styrene, butadiene copolymer 
< 1% 
14807-96-6 
Talc (Mg3H2(SiO3)4) 
< 1% 
13463-67-7 
titanium dioxide 
< 1% 
Full text of each relevant R phrase can be found in heading 16. 
Further Information   
For information purposes: 
(*) Main ingredients: Lithium hexafluorophosphate, organic carbonates 
Because of the cell structure the dangerous ingredients will not be available if used properly. 
During charge process a lithium graphite intercalation phase is formed. 
4. First Aid Measures 
General information 
The following first aid measures are required only in case of exposure to interior battery components after 
damage of the external battery casing. 
Undamaged, closed cells do not represent a danger to the health. 
After inhalation   
Ensure of fresh air. Consult a physician.   
After contact with skin 