9.1.4 Inspection Criteria
9.1.4.1 Cosmetic Inspection (Panel):
Item Judgment Criteria Classification
Chipping on Panel
a
b
c
a
b
a≦3.0mm、b≦3.0mm、c≦t
( Bottom glass thickness)
MA
Scratch on Panel
*Note-2
W≦0.05mm or L< 5mm: Ignored
0.05mm<W≦0.1mm and L≦5mm: N≦5
W>0.1mm or L>5mm: Not allowed
MI
Bubble or Dent on
Panel
*Note-3
D≦0.2mm: Ignored
0.2mm<D≦0.3mm: N≦5
D>0.3mm: Not allowed
MI
Panel Crack
Not Allowed crack
MA
Bezel Deformation Obvious deformation is not allowed. MI
Bezel Oxidation
Not allowed if it rusts continuously over 1 cm (It is out of
warranty with rusted tin plate)
MI
Bezel Scratch L≦20mm , W≦0.2 , N≦3 MI
Metal Squash Dent
/Flange(Front Side)
D(W)≦1,L≦3,N≦3; MI
B/L High Voltage Wire
Denudation
Not allowed MA
Polarizer flaw or leak
out resin
Defect is defined as the active area. MI
Outline Dimension Must in Spec, refer to related product spec. MI