Instructions

11
10. Preheating Method 预热方法
>> >>
>> >>
Method 2
方法2
Notes: The print preheating standard is adjusted at the factory, PLA preheating standard: nozzle temperature 200 °, hot bed temperature 60 °, ABS
preheating standard: nozzle temperature 240 °, hot bed temperature 70 °.If you need to adjust it due to printing materials or other reasons, you can
adjust the parameters on the interface home page control → temperature → PLA / ABS preheat setting.
注意:打印预热参数标准出厂时已调整好,PLA预热标准:喷嘴温度200°,热床温度60°,ABS预热标准:喷嘴温度240°,热床温度70°。若因打印材料或其
他原因需要调整,可以在界面首页控制→温度→PLA/ABS预热设置进行参数调整。