Technical data

TM 9-1005-319-23&P 0015
0015-10
INSPECTION — ACCEPTANCE AND REJECTION CRITERIA - Continued
2 6
1 v s 1 1 5
Figure 15. Inspection of Chamber.
8. If upper receiver and barrel assembly is assembled, inspect chamber using reflector tool (26) and
flashlight. Pits 1/8 in. (0.32 cm) in length are cause for rejection. Replace barrel assembly if defective.
If barrel assembly is replaced, inspect headspace. See TEST AND INSPECTION in this work package.
9. Inspect upper receiver assembly for cracks, corrosion, wear, or damage.
a. Small dents or gouges that do not affect functioning will not be cause for rejection.
b. If upper receiver assembly contains cracks or holes, the upper receiver assembly will be replaced.
END OF TASK
REPAIR OR REPLACEMENT
C O R R O D E D
( R E P A R A B L E )
C O R R O D E D
( N O N R E P A R A B L E )
1 v s 1 1 6
Figure 16. Inspection for Corrosion.
1. Repair corroded upper receiver assembly surface as follows:
a. Sand corroded area with abrasive cloth (WP 0045, item 13) and make sure all corrosion has been
removed.