Post-curing (Mandatory):
Submerge the parts into glycerol/glycerin(CAS # 56-81-5) and start FormCure with 60 ℃ /
30 mins
setting. Wash off glycerol in water and dry off with paper towel.
* If prints don’t sink completely into glycerol, add water (no more than half of volume) to
adjust liquid density.
** If prints are still tacky to touch after post-curing, rinse with acetone (CAS # 67-64-1) for
no more than 1 minute will significantly reduce tackiness.
Storage:
Keep resin away from heat and light.
NOT accessible to children.
Note:
Keep printing environment well ventilated.
Wear gloves when handling Spring resin and avoid direct contact.
Vibration of the parts during printing process might cause resin splash onto printer ’s
cover. Use paper towel and IPA to clean immediately.
Don’t leave the parts on building platform after printing for more than one day.
Spring resin should NOT use with food, drink, or on/in the human body unless
specifically indicated.